PC/ABS 泰國科思創(chuàng)(拜耳) FR2000注塑級
物性表
|
|||||
性能項目 | 測試條件 | 測試方法 | 數(shù)值/描述 | 單位 | |
機(jī)械性能 | 拉伸強(qiáng)度(引張強(qiáng)度) | ASTM D638/ISO 527 | 45 | kg/cm2(MPa)[Lb/in2] | |
斷裂伸長率 | ASTM D638/ISO 527 | >50 | % | ||
拉伸模量 | ASTM D638/ISO 527 | 2700 | kg/cm2(MPa)[Lb/in2] | ||
拉伸屈服伸長率(延伸率) | ASTM D638/ISO 527 | 4 | % | ||
拉伸斷裂伸長率(延伸率) | ASTM D638/ISO 527 | >50 | % | ||
彎曲模量(彎曲彈性率) | ASTM D790/ISO 178 | kg/cm2(MPa)[Lb/in2] | |||
彎曲強(qiáng)度 | ASTM D790/ISO 178 | kg/cm2(MPa)[Lb/in2] | |||
洛氏硬度 | ASTM D785 | ||||
IZOD 缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D256/ISO 179 | N | kg·cm/cm(J/M)ft·lb/in | |
1/4" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
Charpy沖擊強(qiáng)度 | 23℃ (缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||
-30℃(缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
23℃(無缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
-30℃(無缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 1.18 | ||
成型收縮率 | ASTM D955 | 0.7 | % | ||
熔融指數(shù)(流動系數(shù)) | 200℃/5kg | ASTM D1238/ISO 1133 | 26 | g/10min | |
220℃/10kg | ASTM D1238/ISO 1133 | g/10min | |||
吸水率 23℃/24H | ASTM D570/ISO 62 | 0.5 | % | ||
熱性能 | 熱變形溫度 | 退火 | ASTM D648/ISO 75 | 80 | ℃(℉) |
未退火 | ASTM D648/ISO 75 | 90 | ℃(℉) | ||
維卡軟化點 | ASTM D1525/ISO R306 | 93 | ℃(℉) | ||
熔點 | - | 240 | ℃(℉) | ||
燃燒性(率) | UL94 | ||||
線性膨脹系數(shù) | ASTM D696/ISO 11359 | 0.76 | mm/mm.℃ | ||
電氣性能 | 介電常數(shù) | 100HZ | ASTM D150/IEC 60250 | 3.2 | |
1MHZ | ASTM D150/IEC 60250 | 3.1 | |||
體積電阻率 | ASTM D257/IEC 60093 | 1E14 | Ω.cm | ||
表面電阻率 | ASTM D257/IEC 60093 | 1E16 | Ω | ||
耐電弧性 | ASTM D495/IEC 60112 | 350 | |||
加工條件 | 干燥條件 | ||||
加工溫度 | 射嘴 | ℃ | |||
料筒前段 | ℃ | ||||
料筒中段 | ℃ | ||||
料筒后段 | ℃ | ||||
熔體溫度 | ℃ | ||||
模具溫度 | ℃ | ||||
壓力 | 注塑壓力 | Mpa | |||
保壓壓力 | Mpa | ||||
背壓 | Mpa | ||||
螺桿轉(zhuǎn)速 | rpm | ||||
其他 | 備注 | ||||
顏色 | 透明 | ||||
特性 | 汽車零件 | ||||
用途 |