PPS 美國泰科納 1140L4注塑級 物性認(rèn)證數(shù)據(jù)表
性能項(xiàng)目 | 測試條件 | 測試方法 | 數(shù)值/描述 | 單位 | |
機(jī)械性能 | 拉伸強(qiáng)度(引張強(qiáng)度) | ASTM D638/ISO 527 | kg/cm2(MPa)[Lb/in2] | ||
斷裂伸長率 | ASTM D638/ISO 527 | 195 | % | ||
拉伸模量 | ASTM D638/ISO 527 | 14700 | kg/cm2(MPa)[Lb/in2] | ||
拉伸屈服伸長率(延伸率) | ASTM D638/ISO 527 | % | |||
拉伸斷裂伸長率(延伸率) | ASTM D638/ISO 527 | % | |||
彎曲模量(彎曲彈性率) | ASTM D790/ISO 178 | 14500 | kg/cm2(MPa)[Lb/in2] | ||
彎曲強(qiáng)度 | ASTM D790/ISO 178 | kg/cm2(MPa)[Lb/in2] | |||
洛氏硬度 | ASTM D785 | ||||
IZOD 缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D256/ISO 179 | 10 | kg·cm/cm(J/M)ft·lb/in | |
1/4" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
Charpy沖擊強(qiáng)度 | 23℃ (缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||
-30℃(缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
23℃(無缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
-30℃(無缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 1650 | ||
成型收縮率 | ASTM D955 | % | |||
熔融指數(shù)(流動(dòng)系數(shù)) | 200℃/5kg | ASTM D1238/ISO 1133 | g/10min | ||
220℃/10kg | ASTM D1238/ISO 1133 | g/10min | |||
吸水率 23℃/24H | ASTM D570/ISO 62 | % |